First heat the plastic particles at 200 degrees, pull the film out and then check the thickness and cool it, and finally form a roll of film for making bags
The plastic particles are heated 200 degrees first, the film is pulled out, the thickness is detected and cooled, and a roll of film is formed to make the bag.